OK Tigrod 5183 was developed to provide the highest strengths possible in the as welded condition of alloy AA 5083 and other similar high magnesium alloys. The more common OK Tigrod 5356 will typically fail to meet the as-welded tensile requirements of AA 5083. The alloy is typically utilised in marine and structural applications where high strengths, high fracture toughness for impact resistance and exposure to corrosive elements are important. The alloy is not recommended for elevated temperature applications due to its susceptibility to stress corrosion cracking. The alloy is non-heat treatable.
典型拉伸性能
As welded
|
屈服強度
|
延伸率
|
抗拉強度
|
140 MPa
|
25 %
|
290 MPa
|
夏比V型缺口沖擊性能
As welded
|
沖擊值
|
測試溫度
|
90 J
|
20 °C
|
焊縫金屬分析
Mn
|
Cu
|
Zn
|
Ti
|
Si
|
Mg
|
Al
|
Cr
|
Fe
|
0.65 %
|
0.01 %
|
0.01 %
|
0.100 %
|
0.04 %
|
4.9 %
|
94.200 %
|
0.08 %
|
0.13 %
|
認證:
|
R 5183, ABS, EN 13479, CE, A5.10/A5.10M:2012 ER5183, CWB, 61.039.04, DB, JIS Z 3232, JIS, 3.2MM, NAKS/HAKC, 04667, VdT?V
|
分類:
|
R5183, SFA/AWS A5.10, Wire Electrode, S Al 5183 (AlMg4,5Mn0,7(A)), EN ISO 18273, Wire Electrode, A5183, JIS Z 3232, Wire Electrode
|
認證均基于工廠的所在地。如需更多信息,請聯(lián)系伊薩。
|