Bare, corrosion-resistant, chromium-nickel-molybdenum welding rods for welding austenitic stainless alloys of the 19% Cr, 9% Ni, 3% Mo types. OK Tigrod 317L has good resistance to general corrosion and pitting due to its high content of molybdenum. The alloy has a low carbon content which makes it particularly recommended when there is a risk of intergranular corrosion. The alloy is used in severe corrosion conditions such as in the petrochemical, pulp and paper industries.
典型拉伸性能
As welded
|
屈服強度
|
延伸率
|
抗拉強度
|
390 MPa
|
45 %
|
600 MPa
|
夏比V型缺口沖擊性能
As welded
|
沖擊值
|
測試溫度
|
135 J
|
20 °C
|
55 J
|
-196 °C
|
焊縫金屬分析
Mn
|
Mo
|
Cu
|
C
|
Si
|
FN WRC-92
|
Ni
|
N
|
Cr
|
1.4 %
|
3.6 %
|
0.05 %
|
0.01 %
|
0.4 %
|
7 %
|
13.6 %
|
18.9 %
|
分類:
|
W18 15 3 L, EN ISO 14343-A, Wire Electrode, ER317L, SFA/AWS A5.9, Wire Electrode
|
合金類型:
|
Austenitic (with approx. 8 % ferrite) 19% Cr - 12% Ni - 3% Mo - Low C
|





|